Built from archived notes on rub, light and wash fastness testing for printed bags, plus the factory checkpoints behind each grade.
The sample came back in a courier envelope with a sticky note on the front: print rubbed off on the white shirt underneath. The buyer had approved that print twice, once on screen and once in hand, and neither approval had asked the ink to survive a warm afternoon against cotton.
That note is where the real invoice starts. The unit price on the quotation covers fabric, printing, sewing and packing. It does not cover the four costs that follow a print which moves, fades or bleeds, and those four costs are usually larger than the test that would have caught the problem. This piece takes a printed bag order apart line by line and puts a number against each fastness gap, so a buyer can see which test earns its fee first.
The Quote With Four Lines and One Missing One

A typical printed bag quotation arrives with four visible lines: material, print, labour and packing. Each line is negotiable, and buyers spend most of their time there. The missing line is the one that decides whether the other four hold, and it is the fastness line.
Nothing on that sheet says which rub, light or wash method was run, at what grade, on which colorway. A supplier can print beautifully and still ship a bag that marks a shirt in the first week. The quotation looks complete because the cost of that failure sits outside it, on the buyer’s side of the table.
Splitting the hidden cost into parts makes the choice easier. Four items usually account for most of it: rework at the factory, claims and markdowns after arrival, downgraded stock that sells at a discount, and expedited freight when replacement has to fly. A fifth, the test fee itself, is the smallest of the group and the only one a buyer can budget in advance.
Rework: What a Failed Wet Rub Adds to the Unit Price

Crocking is the trade word for colour transfer by rubbing, and it produces complaints faster than any other print fault. A wet sleeve against a fresh print, a white shirt against a bag carried under the arm, and the colour moves. Rub tests reproduce this with a standard counterface rubbed dry and wet across the printed surface, graded on a gray scale for staining and for colour change.
When a wet rub fails, the rework is not a wipe and a reprint. Printed panels are usually cut and sewn by then, so the fix means remaking panels, reprinting, resewing and rechecking. Each of those steps carries its own labour, and the material already consumed is lost. The unit price on the reorder quietly absorbs all of it.
The pass bands belong in the purchase order rather than in a conversation. On bags carried against clothing, dry rub at grade 4 and wet rub at grade 3 or better are common commercial requirements. Those numbers give the factory a target and give the buyer a basis for rejection, and neither side has to argue about what “good” means.
Claims and Markdowns: The Cost That Arrives After the Container
A claim rarely arrives as a single email. It arrives as photographs from a store, a request for credit, and a quiet decision not to reorder. The credit note is the visible part. The lost reorder is the larger part, and it never appears on any document.
Markdowns work the same way. Stock that has faded or marked gets reduced to clear, and the difference between full and reduced price is a cost the buyer carries. On a seasonal programme, that difference can exceed the entire printing cost of the run.
Cure sits behind many of these claims. Prints that cure properly bond the pigment to the fabric. Prints rushed off an underheated dryer pass the visual check at the factory and fail the first wet shirt in the field. The factory sees a clean bag under its own lights. The customer sees a mark on a sleeve two weeks later.
Light Fastness: Paying Once for a Window Display You Cannot Recall

A bag that sits in a shop window for a summer is doing exactly the job the brand bought it for. Ultraviolet exposure fades unstable pigments over weeks, and the faded stock is unsellable even though every bag is structurally perfect. The cost here is not a defect. It is a display that worked against the product.
Light fastness testing predicts that behaviour before the run. Exposure tests rate fading on blue wool or numeric scales, and bags intended for window display or outdoor use should carry a stated light rating instead of an assumption. The fee is paid once, at the sample stage, and it covers every unit in the window.
The calculation is simple when the display is planned. Count the units that will sit in direct sun, multiply by the retail price, and compare that figure with the cost of one exposure test on the ink system. On any programme with a window plan, the test is the cheaper line by a wide margin.
Wash Fastness and the Reusable Bag Promise
Reusable bags make a promise the customer will test at home. Wash fastness separates prints that survive repeated laundering from prints that bleed in the first cold wash, and the gap between those two outcomes is a customer who keeps the bag and one who quietly stops using it.
The buyer’s job is to name the method, the number of cycles and the pass grade. “Colourfast” without a method is a promise with no measurement behind it, and it gives the factory nothing to test against. A stated cycle count turns the promise into a specification.
This matters most for grocery and retail programmes where the bag is expected to return week after week. A print that bleeds onto a light garment in the wash creates a complaint about the bag and about the brand that gave it away. The test fee is small next to the cost of that complaint repeated across a season.
Cure Temperature and Line Speed as Cost Variables

Ink chemistry, cure and fabric interact at the printing stage, and the fastness tests measure what that stage decided. Cure is the biggest variable of the three. Properly cured inks bond. Rushed cures look fine on the line and fail the first rub or wash.
Cure temperature and line speed belong on the spec sheet for that reason. When line speed rises, dwell time in the dryer falls, and the ink may not reach the bond it needs. A factory running to a deadline has an incentive to speed up. A spec that names the cure window removes that incentive from the argument.
For the buyer, this is a cost variable rather than a technical footnote. Every hour saved on the dryer is paid for later in rework, claims or markdowns, and the later payment is always the larger one. Naming the cure window costs nothing at the quotation stage.
Adding the Test Lines to the Order Without Adding Waste
Three lines in the purchase order convert fastness from hope into contract. The first names the methods: print fastness tested per named methods on each colorway, with reports issued alongside the shipment. The second states the grade bands per test, dry rub 4 and wet rub 3 minimum, or whatever values the programme has agreed. The third retains a golden sample approved under store-equivalent lighting as the visual reference for disputes.
The third line does the most work in practice. Fastness grades are laboratory numbers, and customers judge bags in daylight. The golden sample bridges the two, and reorders are checked against it before shipment. Visual colour appraisal under controlled illumination follows the same logic as ASTM D1729, the standard practice for appraising colour differences under controlled lighting.
None of this adds material waste. A test consumes a few printed pieces, not a production run, and the reports travel with the shipment. The waste a buyer should worry about is the rework that happens when no line was written at all.
How to Read a Fastness Report Before You Pay the Balance

A report that arrives without a method name is not a report. The first check is whether each test names its standard, its exposure or cycles, and the colorway it covers. A single grade for the whole order hides the colour that actually failed.
The second check is the grading scale. Rub results should be stated on the gray scale for staining and for colour change, and light results on the stated scale for the ink system. Numbers without a scale cannot be compared with the bands in the order.
The third check is the sample link. The report should point to the approved sample and the colorway it represents, so the balance payment rests on evidence rather than on a conversation. When those three checks pass, the fastness line has done its job and the hidden costs stay hidden.
FAQ
Is a rub test enough if the bag never goes in a washing machine?
For a bag that only travels against clothing and hands, dry and wet rub cover the main risk. Wash fastness matters when the bag is reusable and the customer is likely to launder it. Light fastness matters when the bag will sit in a window or outdoors. The test set follows the use, not the product category.
Why does the same print grade differently on two fabric colours?
The base fabric changes how the ink reads and how staining shows on the gray scale. A dark ground can mask transfer that a light ground reveals. This is why grade bands belong per colorway rather than per order, and why a single report line for a multi-colour programme is not enough.
Can a factory test fastness on the bulk run instead of the sample?
Testing on bulk tells you what you have already made. Testing on the sample tells you what you are about to make. A bulk test still has value as a shipment check, but it cannot prevent the rework, because the panels are already printed and cut by then.
What does a golden sample do that a grade number cannot?
A grade number describes a laboratory result under controlled light. A golden sample shows what the approved print looks like in the lighting a customer will actually stand in. When a dispute arises, the retained sample settles the question faster than any report, and reorders can be checked against it before the container seals.